Rebuild Resin 1 & 4 Hour Cartridges

​

  1. Mount cartridge into applicator gun.  Ensure the smaller tube for the 3:1 cartridge (Rebuild 4 Hour) is lined up with the smaller piston of the gun

  2. Remove cap on the end of the cartridge

  3. Pump the required amount of product onto the mixing board

  4. Discard any excess base or activator which may extrude initially

  5. Mix thoroughly with a scraper, using a folding action until streak free

  6. Appy resin to where you want to bond your timber

  7. Leave slightly proud, so can be sanded down once cured

​